Mechanical Properties Metric English Comments
Peel Strength 1.09 kN/m

@Thickness 0.0508 mm
6.20 pli

@Thickness 0.00200 in
IPC-TM-650 2.4.8
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material
SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a ..