Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 7.01 kN/m @Temperature 22.2 °C |
40.0 pli @Temperature 72.0 °F |
Bell Peel |
Hexcel® Redux® 319 High Performance Modified Epoxy Film Adhesive (0.07 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |