Polymer Property : Peel Strength = 76.5 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 13.4 kN/m

@Temperature 24.0 °C
76.5 pli

@Temperature 75.2 °F
Metal-to-metal
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel
Peel Strength 13.4 kN/m

@Temperature 82.0 °C
76.5 pli

@Temperature 180 °F
Metal-to-metal
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel