Ball Indentation Hardness 75.0 MPa

@Load 36.5 kg
10900 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored
Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper..
Ball Indentation Hardness 75.0 MPa

@Load 36.5 kg
10900 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored
Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac..
Ball Indentation Hardness 75.0 MPa

@Load 36.5 kg
10900 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored
High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration..