Polymer Property : Ball Indentation Hardness = 23200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 160 MPa

@Load 36.5 kg
23200 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Ball Indentation Hardness 160 MPa

@Load 36.5 kg
23200 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Ball Indentation Hardness 160 MPa

@Load 36.5 kg
23200 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MT30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..