Mechanical Properties Metric English Comments
Fatigue Strength 105 MPa

@# of Cycles 1.00e+6
15200 psi

@# of Cycles 1.00e+6
1 Hz
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..