Polymer Property : Fatigue Strength = 132000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 910 MPa

@# of Cycles 1.00e+7
132000 psi

@# of Cycles 1.00e+7
Smooth (Kt = 1); Stress Ratio = 0.1; Axial Loading
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4984
High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4984.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi..