Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 245 MPa @# of Cycles 1.00e+7 |
35500 psi @# of Cycles 1.00e+7 |
|
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Fatigue Strength | 245 MPa @# of Cycles 1.00e+7 |
35500 psi @# of Cycles 1.00e+7 |
|
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Fatigue Strength | 245 MPa @# of Cycles 1.00e+7 |
35500 psi @# of Cycles 1.00e+7 |
|
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Fatigue Strength | 245 MPa @# of Cycles 1.00e+7 |
35500 psi @# of Cycles 1.00e+7 |
|
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Fatigue Strength | 245 MPa @# of Cycles 1.00e+7 |
35500 psi @# of Cycles 1.00e+7 |
|
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Fatigue Strength | 245 MPa @# of Cycles 1.00e+7 |
35500 psi @# of Cycles 1.00e+7 |
|
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |