Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 180 MPa | 26100 psi | endurance limit; test conditions not reported |
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800) AL 348 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Fatigue Strength | 180 MPa | 26100 psi | endurance limit; test conditions not reported |
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100) AL 321 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Fatigue Strength | 180 MPa | 26100 psi | endurance limit; test conditions not reported |
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700) AL 347 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |