Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength >= 275 MPa

@# of Cycles 1.00e+7
>= 39900 psi

@# of Cycles 1.00e+7
(R=-1)
Schmolz + Bickenbach MoldMAX® V Copper Alloy
Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores ..
Fatigue Strength 275 MPa
39900 psi
Drawn rod and bar
CMW® 100 Copper Alloy
CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther..