Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 320 - 380 MPa @# of Cycles 1.00e+8 |
46400 - 55100 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 190 Strip; SHM (TM05) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 320 - 390 MPa @# of Cycles 1.00e+8 |
46400 - 56600 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R.. |