Polymer Property : Fatigue Strength = 330 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 290 - 330 MPa

@# of Cycles 1.00e+8
42100 - 47900 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 290 - 330 MPa

@# of Cycles 1.00e+8
42100 - 47900 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..