Polymer Property : Fatigue Strength = 35000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 241 MPa
35000 psi
Strip (TH04)
CMW® 100 Copper Alloy
CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther..
Fatigue Strength 241 MPa
35000 psi
Rod & Bar
CMW® 73 Copper Alloy
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w..
Fatigue Strength 241 MPa
35000 psi
endurance limit; test details not reported
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..