Mechanical Properties Metric English Comments
Fatigue Strength 260 - 300 MPa

@# of Cycles 1.00e+8
37700 - 43500 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 3 Strip; AT (TF00) Temper (UNS C17510)
Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 94%Stress Relaxation after 1000 hrs @ 200°C: 72%Formability Ratio..