Mechanical Properties Metric English Comments
Fatigue Strength 52.0 MPa

@# of Cycles 1.00e+6
7540 psi

@# of Cycles 1.00e+6
1 Hz
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..