Fatigue Strength 38.0 MPa
5510 psi
Average value: 38.0 MPa Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..