Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 414 MPa @# of Cycles 1.00e+6 |
60000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T3 AT110 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Fatigue Strength | 414 MPa @# of Cycles 1.00e+6 |
60000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T3 AT120 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Fatigue Strength | 414 MPa @# of Cycles 1.00e+6 |
60000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Fatigue Strength | 414 MPa @# of Cycles 1.00e+6 |
60000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T3 AT90 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Fatigue Strength | 414 MPa @# of Cycles 1.00e+6 |
60000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T3 AT110 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Fatigue Strength | 414 MPa @# of Cycles 1.00e+6 |
60000 psi @# of Cycles 1.00e+6 |
R = -1, 105 ksi YS |
Materion ToughMet® T3 AT90 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |