Polymer Property : Fatigue Strength = 8700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 60.0 MPa

@# of Cycles 1.00e+6
8700 psi

@# of Cycles 1.00e+6
1 Hz
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..