Polymer Property : Fatigue Strength = 97200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 610 - 670 MPa
88500 - 97200 psi
Limit; test specifics not reported
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged
High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i..