Polymer Property : Dart Drop, Total Energy = 10.62 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 10.62 J

@Thickness 3.20 mm
7.833 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1200-03 Polycarbonate Resin
Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...