Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | >= 20.3 J | >= 15.0 ft-lb | ASTM D3029 |
S&E Specialty Polymers GPP1001V0M-HCO-15 PP Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high lev.. |
|||
Dart Drop, Total Energy | >= 20.3 J | >= 15.0 ft-lb | ASTM D5420 |
S&E Specialty Polymers GPP1001V0M-HCO PP Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high level of flam.. |