Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 2.44 - 2.71 J | 1.80 - 2.00 ft-lb | Average value: 2.53 J Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | ASTM D3420 |
LyondellBasell Alathon® L4903 High Density Polyethylene ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | ASTM D3420 |
LyondellBasell Alathon® L5906 High Density Polyethylene ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | ASTM D4272 |
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | ASTM D4272 |
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | ASTM D4272 |
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | ASTM D4272 |
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Dart Drop, Total Energy | 2.44 J | 1.80 ft-lb | Average value: 2.44 J Grade Count:4 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |