Polymer Property : Dart Drop, Total Energy = 31.7 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
Dart Drop, Total Energy 43.0 J
31.7 ft-lb
SABIC Method
SABIC Innovative Plastics Lexan® FL920 PC
Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm).
Dart Drop, Total Energy 43.0 J
31.7 ft-lb
SABIC Method
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific)
Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm).
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS
PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management.
Dart Drop, Total Energy 43.0 J
31.7 ft-lb
ASTM D3763
Techmer ES Plastiblend® PC/ABS FR 1950 BK
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Dart Drop, Total Energy 43.0 J
31.7 ft-lb
ASTM D3763
Techmer ES Plastiblend® PC/ABS FR 2810
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY FXW751SK ASA+PC
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD4471 PC
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific)
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East)
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..