Mechanical Properties Metric English Comments
Dart Drop, Total Energy 58.7 J
43.3 ft-lb
ASTM D3763
Techmer ES Plastiblend® PC/ABS FR 6206 UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Dart Drop, Total Energy 58.7 J
43.3 ft-lb
ASTM D3763
Techmer ES Plastiblend® PC/ABS FR 6209
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.