Mechanical Properties Metric English Comments
Dart Drop, Total Energy 89.3 J
65.9 ft-lb
ASTM D3763
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..
Dart Drop, Total Energy 89.3 J
65.9 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin
Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip..