Polymer Property : Multi-axial Impact @ -30°C Total Energy = 23.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Multi-axial Impact @ -30°C Total Energy 23.8 J
17.6 ft-lb
ASTM 3763; at 2.2 m/sec, 100% ductile
S&E Specialty Polymers TufFill™ 5004UV Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..