Mechanical Properties Metric English Comments
Falling Dart Impact 0.447 J
0.330 ft-lb
ASTM D3029
Total 620 Polystyrene  (discontinued **)
Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high ..