Polymer Property : Falling Dart Impact = 10.41 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 14.11 J
10.41 ft-lb
ASTM D3029
Total PSI 825E Polystyrene
Polystyrene 825E is a high impact polystyrene designed specifically for extrusion/thermoforming. Over the years, this popular resin has established itself as the standard extrusion grade high impact..
Falling Dart Impact 14.11 J
10.41 ft-lb
ASTM D3029
Total PSI 830 Polystyrene
Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m..
Falling Dart Impact 14.11 J
10.41 ft-lb
ASTM D3029
Total PSI 825 Polystyrene
Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such ..