Mechanical Properties Metric English Comments
Falling Dart Impact 14.68 J
10.83 ft-lb
ASTM D3029
Total 819E Polystyrene  (discontinued **)
Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof..