Polymer Property : Falling Dart Impact = 11.3 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 11.3 - 16.1 J
8.33 - 11.9 ft-lb
Average value: 13.5 J Grade Count:8
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
Falling Dart Impact 11.3 J
8.33 ft-lb
ASTM D3763
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe..
Falling Dart Impact 11.3 J
8.33 ft-lb
ASTM D3029
Total PSI 625 Polystyrene
Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi..
Falling Dart Impact 11.3 J
8.33 ft-lb
ASTM D3029
Total PSI 975E Polystyrene
Polystyrene 975E is a high impact polystyrene designed for extrusion/thermoforming applications. The food ESCR properties of 975E dictate its use for dairy applications that are subjected to high bu..