Mechanical Properties Metric English Comments
Falling Dart Impact 10.8 - 20.6 J
8.00 - 15.2 ft-lb
Average value: 14.9 J Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..