Polymer Property : Falling Dart Impact = 15.5 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 21.0 J
15.5 ft-lb
@ 23°C, 3.4 m/s; ASTM D3763
Dow INSPIRE™ D500.00 Developmental Performance Polymer
D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applicat..