Mechanical Properties Metric English Comments
Falling Dart Impact 15.6 J
11.5 ft-lb
ASTM D3763
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..