Polymer Property : Falling Dart Impact = 16.9 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 16.9 J
12.5 ft-lb
ASTM D3029
Total PSI 935E Polystyrene
Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and..
Falling Dart Impact 16.9 J
12.5 ft-lb
Total PSI 940E Impact Polystyrene
Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination of high gl..