Polymer Property : Falling Dart Impact = 187 J
Polymer Property :
Falling Dart Impact =
187 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Falling Dart Impact
187
J
138
ft-lb
73°F; ASTM D3029
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.