Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 3.00 - 27.0 J @Temperature -30.0 - -30.0 °C |
2.21 - 19.9 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 13.1 J Grade Count:5 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |
|||
Falling Dart Impact | 3.00 - 27.0 J @Thickness 3.17 - 3.17 mm |
2.21 - 19.9 ft-lb @Thickness 0.125 - 0.125 in |
Average value: 13.1 J Grade Count:5 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |