Polymer Property : Falling Dart Impact = 21.4 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 29.0 J
21.4 ft-lb
-29°C; Private Lab
Polymer Industries Densetec PP Copolymer Sheet
Polymer Industries’ Densetec Copolymer Propylene differs from the Densetec Homopolymer Polypropylene by virtue of an additional monomer in the product, thus making it a copolymer material. This is ..