Mechanical Properties Metric English Comments
Falling Dart Impact 30.0 J
22.1 ft-lb
0.5" tup, 150"/sec, at -30°C, injection molded specimen; ASTM D3763
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant  (discont
Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. ..
Falling Dart Impact 30.0 J
22.1 ft-lb
0.5" tup, 150"/sec, at -30°C, injection molded specimen; ASTM D3763
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant  (disconti
Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. ..