Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 33.0 J | 24.3 ft-lb | @ 0°C, 6.7 m/s; ASTM D3763 |
Dow INSPIRE™ D7030EZ Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |