Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 4.34 - 7.57 J | 3.20 - 5.58 ft-lb | Average value: 5.62 J Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |