Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | >= 3.43 J @Temperature 23.0 °C |
>= 2.53 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPC SK3005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Falling Dart Impact | >= 3.43 J @Temperature 23.0 °C |
>= 2.53 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPC TC3005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |