Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 4.50 - 15.1 J | 3.32 - 11.1 ft-lb | Average value: 8.17 J Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Falling Dart Impact | 4.50 J | 3.32 ft-lb | ASTM D3763 |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |