Polymer Property : Falling Dart Impact = 8.41 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 6.21 - 11.4 J
4.58 - 8.41 ft-lb
Average value: 8.11 J Grade Count:9
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..