Polymer Property : Falling Dart Impact = 8.70 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 11.8 J
8.70 ft-lb
ASTM D3763
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant  (discontinu
Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; ..