Mechanical Properties Metric English Comments
Falling Dart Impact 9.04 - 583 J
6.67 - 430 ft-lb
Average value: 63.3 J Grade Count:21
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Falling Dart Impact 9.04 J
6.67 ft-lb
ASTM D3029
Total 965E Polystyrene  (discontinued **)
Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially desig..
Falling Dart Impact 9.04 J
6.67 ft-lb
73°F; ASTM D3029
Spartech SP-2010 HIPS Polystyrene Sheet
Description: Polystyrene SheetInformation provided by Spartech.
Falling Dart Impact 9.04 J
6.67 ft-lb
73°F; ASTM D3029
Spartech SP-2050 Glossy HIPS Polystyrene Sheet
Description: Polystyrene SheetInformation provided by Spartech.