Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 393 MPa
57000 psi
Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal
Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-35All information provided by Pacific Sintered Metals.
Tensile Strength, Ultimate 393 MPa
57000 psi
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S Powdered Metal
Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-35Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Ultimate <= 393 MPa
<= 57000 psi
Eagle Brass 18665 MSP1, Annealed
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Tensile Strength, Ultimate 393 - 455 MPa
57000 - 66000 psi
Eagle Brass 220 Commercial Bronze, Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Tensile Strength, Ultimate 393 - 462 MPa
57000 - 67000 psi
Eagle Brass 230 Red Brass, 3/4 Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 393 - 462 MPa
57000 - 67000 psi
Eagle Brass 260 Cartridge Brass, 1/2 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Ultimate 393 - 476 MPa
57000 - 69000 psi
Eagle Brass 425 Tin Brass 2%, 1/2 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Ultimate 393 - 517 MPa
57000 - 75000 psi
Eagle Brass 762 Nickel Silver 12%, Annealed
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
Tensile Strength, Ultimate 393 MPa

@Temperature 649 °C
57000 psi

@Temperature 1200 °F
Tempering Temperature-1200°F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..
Tensile Strength, Ultimate 393 MPa

@Temperature 649 °C
57000 psi

@Temperature 1200 °F
ASTM E8
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..