Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-35All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.80 - 7.20 g/cc
0.246 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 70
70
Apparent
Tensile Strength, Ultimate 393 MPa
57000 psi
Tensile Strength, Yield 276 MPa
40000 psi
Elongation at Break 1.0 %
1.0 %
Modulus of Elasticity 131 GPa
19000 ksi
Flexural Strength 689 MPa
100000 psi
Transverse Rupture
Charpy Impact, Unnotched 6.78 J
5.00 ft-lb