Tensile Strength, Ultimate 0.04474 MPa

@Temperature 150 °C
6.489 psi

@Temperature 302 °F
ASTM #1 Oil Immersion for 70 hours; ASTM D412 Die C
Freudenberg Simrit S80 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..