Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.590 MPa
85.6 psi
ASTM D 638
REXtac Rextac® RT 2732 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good tack, and very long open timeApplications: Component of hot mel..