Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.689 MPa | 100 psi | 2.4 pcf density |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |
|||
Tensile Strength, Ultimate | 0.689 - 57.0 MPa | 100 - 8270 psi | Average value: 11.3 MPa Grade Count:258 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |